Chemical composition, %
C Cr Ni Mg Mo Fe
≤0.08 17.0~21.0 50~55 ≤0.01 2.8~3.30 Margin
Nb B S Mn Si P
4.75~5.50 ≤0.006 ≤0.015 ≤0.35 ≤0.35 ≤0.015
Cu Ti: Al V Ca Co
≤0.30 0.65~1.15 0.30~0.7 - ≤0.01 ≤1.00

Mechanical properties of GH4169 alloy at room temperature
Yield Strength Tensile strength Elongation Brinell hardness
Mpa,≥ Mpa,≥ %,≥ HB
550 965 30 ≤363

GH4169 Physical properties
Density Melting point Melting temperature range Magnetic properties
g/cm3 ℃ ℃  
8.24 1260~1340 1260~1320 Non

GH4169 specific heat capacity
θ/℃ 300 400 500 600 700 800 900 1000
c/(J/(kg·C)) 481.4 493.9 514.8 539.0 573.4 615.3 657.2 707.4

GH4169 linear expansion coefficient

GH4169 Thermal conductivity


GH4169 is a Fe-Ni-Cr based precipitation hardening deformation high temperature alloy. The long-term use temperature range is -253~650℃, and the short-term use temperature is 800℃. It has high strength, high toughness and high and low temperature toughness below 650℃. It is resistant to oxidation and corrosion. And has good processing performance and welding performance and long-term structural stability. It can manufacture various parts with complex shapes and is widely used in the above-mentioned temperature range of aerospace, nuclear energy, petroleum industry and extrusion dies. superalloy GH4169 Inconel718 rod nickel-based alloy bar product details